Tuesday, January 22, 2013
artificial grass playground a few technical maintenance knowledge
artificial grass playground a few technical maintenance knowledge
Grass fibers fade and change color?
1, the quality of the grass fiber failure, for example, anti-ultraviolet (UV) agent, anti-aging (amine) the amount of agent added is too small;
The grass fiber recipe unscientific, some of the poor quality of many additives;
Synthetic grass fiber production equipment is backward, poor technology, physical properties of instability;
Environmental impact, such as parts of the strong ultraviolet radiation, acid rain corrosion, industrial pollution.
, Artificial turf fiber fuzz, pilling and chalking?
1, because the higher the frequency of use of the school, poor quality of reticular fibers in 1-2 years, the quality is better in 4-5 years will be different degrees of grass fiber splits 50-60 roots phenomenon of small wire;
PP fiber itself is relatively hard, crisp, easy to fluff and pilling.
, Grass fiber shedding and hair loss?
Production poor, the artificial grass bottom cloth, glue poor quality, resulting in poor overall binding force on the grass;
2, using low-end grass grass fibers (PP material), use grass line from disconnect;
3, the excipients used unqualified (quartz sand particles is too large, not round), causing damage to the grass.
Artificial grass at the bottom of corruption, cracking?
1, artificial turf thin at the bottom, and the general PP material;
2, the bottom of the glue of poor quality or poor gluing process, too much is too thick;
3, venues foundation rugged to be ineligible on the basis of the end of the artificial grass cloth injury;
4, the basis of the overall poor drainage, base cloth a long soak in water.
Five venue artificial grass uneven color, the color difference is serious?
The 1 Synthetic Grass fiber quality is poor, uneven thickness, color instability, easy to cause a different color;
2, site installation poorly designed, scene accessories populate rugged, produce visual color difference;
Venues foundation uneven seams obvious traces;
4, filling excipients failed, the contaminated surface layer;